Ce0.8Gd0.2O1.9-Sr1.95Pr0.05Fe1.5Mo0.5O6-δ heterogeneous structure composite electrolyte for solid oxide fuel cells

Sr1.95Pr0.05Fe1.5Mo0.5O6-δ (SPFM) powder synthesized by combustion method was uniformly compounded with Ce0.8Gd0.2O1.9 (GDC) powder obtained by sol-gel route to prepare GDC-SPFM heterogeneous structure composite electrolytes with 10, 15, 20 and 30 wt.% of SPFM. The crystal structure, micro-morpholog...