INFLUENCE OF GAS GAP ON EFFICIENCY OF COOLING AND MICROSTRUCTURE OF CASTINGS AT FOUNDING OF SILUMINS IN METAL WATER-COOLED MOULD

Increase by 30–40% the linear speed of solidification of ingot with diameter 100 mm, to produce the castings with eutectic modified microstructure.

Saved in:
Bibliographic Details
Main Authors: V. Ju. Stetsenko, R. V. Konovalov
Format: Article
Language:English
Published: Belarusian National Technical University 2010-09-01
Series:Литьë и металлургия
Online Access:https://lim.bntu.by/jour/article/view/797
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:Increase by 30–40% the linear speed of solidification of ingot with diameter 100 mm, to produce the castings with eutectic modified microstructure.